Info
Guides, data and definitions
Sodium-ion is new enough that most of the questions are still technical: which cell for a cold chassis, why a 40C pouch cell is only 5C at −40 °C, what a BMS threshold should be. This is where we keep the answers — data you can check, not brochure copy.
Guides & notes
Data Centre BBU and Rack Backup — Sodium-ion Short Duration
Rack-level backup units for AI and edge data centres — high rate for seconds, hot aisles and the design questions that decide it.
Warehouse AMR and Shuttle Battery — Sodium-ion for Logistics Robots
Packs for AMRs, AGVs, shuttle carts and sorting robots: 24-hour operation, opportunity charging and tens of thousands of shallow cycles.
Electric Tractor and Agricultural Robot Battery — Sodium-ion
Packs for electric tractors, field robots and orchard platforms — heavy continuous loads, dust, and charging in a farmyard with a weak supply.
Robotic Mower Battery — Sodium-ion for Outdoor Power Equipment
Packs for robotic mowers, commercial OPE and garden robots — daily cycles, outdoor charging bases and a battery that sits outside all year.
Cordless Power Tool Battery — High-Rate Sodium Cells
Cells for cordless drills, angle grinders, saws and professional tool packs — 18 V and 36 V platforms, high pulse current and cold sites.
Electric Tug and Harbour Vessel Battery — Sodium-ion
Storage for electric tugs, harbour craft and port workboats — short high-power manoeuvres, salt exposure and berth charging.
Electric Ferry Battery — Sodium-ion for Short-Sea Routes
Storage for short-sea ferries and inland waterway vessels — shore charging windows, cold water and the weight that changes stability.
Electric Bus Battery — Sodium-ion for City Fleets
Packs for city buses and shuttle fleets — depot charging in a fixed window, cold-morning operation and predictable route duty.
Island Microgrid Battery — Sodium-ion for Remote Communities
Storage for island microgrids and remote settlements — diesel displacement, corrosion, sizing by fuel saved and where the economics fail.
Cells & chemistry
Every cell we stock is sodium-ion with a hard-carbon anode and one of three cathodes: layered oxide (higher energy, NCM-like voltage), Prussian white (lower cost, long cycle life) or polyanionic (NFPP — flat voltage, very long life, lower energy). The cathode decides the voltage curve and the cycle life; the form factor decides the current path.
Packs & BMS
A sodium pack is not a lithium pack with different cells. The BMS thresholds differ (over-charge near 4.2 V on oxide, 3.65 V on Prussian white), balancing starts higher, and the low-temperature charge limit is the figure that decides whether a winter application works. Current path, busbar sizing and compression are covered on the product pages; this section collects the rules of thumb.
Enclosure & thermal
Sodium cells run warmer than LFP at the same C-rate on oxide cathodes, and the pack still has to survive a cold soak. Three materials do most of the work: aerogel for the thin thermal barrier between cells, mica for anything near a hot surface, and silicone foam for compression and sealing.
Documents & transport
Cells ship as Class 9 dangerous goods unless they are excepted. The paperwork that actually gets checked at the port is the UN38.3 test summary, the MSDS and the packing instruction on the air waybill. Our quality page lists what arrives with every shipment, and what we do not test in-house.
Definitions
- Continuous C-rate
- The current a cell will hold without a cooling plate, quoted at 20–25 °C and divided by its capacity. A pulse rating is not the same number and is marked as such on the product page.
- First coulombic efficiency
- Charge out divided by charge in on the first cycle. In sodium-ion it tells you how much sodium the hard carbon consumes forming the SEI — a low figure means the anode is eating capacity you paid for.
- Cycle life to 80%
- Capacity at the stated C-rate, temperature and preload until it falls to 80% of the initial value. Any cycle figure without those conditions cannot be compared with another supplier's.
- Derating
- The lower current a cell will accept at low temperature. Charging below 0 °C is limited by sodium plating on the anode, not by the electrolyte freezing.
- Compression (preload)
- The stack pressure a prismatic cell needs to keep its cycle life. Too little and the electrode stack loosens; too much and the separator is crushed.